Inconel 602CA
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 602ca in China. If you're going to wholesale high quality inconel 602ca made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Introduction
Solid Solution
Strengthened Alloy
Nickel
Chromium
Iron
Corrosion
Resistance
90
Mechanical
Behavior
67
Purity
94
Overview
As a leading supplier & manufacturer in China, AEETHER supply cost-effective Inconel 602CA Products.
INCONEL 602CA (UNS N06025 / W.Nr. 2.4633) is one of the most oxidation resistant nickel alloys available. Outstanding oxidation resistance is achieved through a high chromium content (25%) supplemented with aluminum (2.2%) and a microalloying addition of yttrium (0.1%). High chromium contents are known to be beneficial for resisting oxidation. The aluminum addition allows for the formation of a continuous homogenous self repairing AI2O3 subscale. The addition of yttrium improves the adhesion and spalling resistance of the chromium and aluminum oxide scales. The extremely low scaling rate of alloy 602CA makes it an excellent candidate for applications such as calciners, where minimal contamination from scaling is permissible.
Extended exposure to methane (CH4), carbon monoxide (CO), and other carbon rich gases can lead to carburization. As heat resistant alloys absorb carbon, their ductility will gradually decrease. Alloys that are high in nickel, such as alloy 602CA possess excellent resistance to carburization attack8. Alloy 602CA forms a tenacious oxide scale, which provides increased protection from carburization. This protective scale impedes the carbon from being absorbed into the base metal.
Main Standards
ASTM B167
Seamless Pipe & Tube
ASTM B829
Seamless Pipe & Tube
ASTM B775
Welded Pipe
ASTM B751
Welded Tube
ASTM B366
Welded Fittings
ASTM B166
Rod, Bar and Wire
ASTM B168
Plate, Sheet and Strip
ASTM B906
Plate, Sheet and Strip
AWS A5.14 ERNiCrFe-12
Filler Metal
AWS A5.11 ENiCrFe-12
Welding Electrode
Chemical Composition
Data Sheet
Physical Properties
| Density | g/cm3 | 7.93 | |
|---|---|---|---|
| lb/in.3 | 0.29 | ||
| Melting Range | °F | 2444 - 2552 | |
| °C | 1340 - 1400 | ||
Mechanical Properties
| Condition & Size | Tensile Strength | Yield Strength (0.2% Offset) |
Elongation | Reduction of Area | Hardness |
|---|---|---|---|---|---|
| MPa, min | MPa, min | %, min | %, min | Rockwell | |
| Seamless Pipe & Tube | |||||
| Hot-worked annealed or cold worked annealed (all sizes) | 680 | 270 | 30 | ... | ... |
| Rod & Bar | |||||
| Hot-worked annealed or cold worked annealed (all sizes) | 680 | 270 | 30 | ... | ... |
| Plate, Sheet & Strip | |||||
| Annealed | 680 | 270 | 30 | ... | ... |
More +





FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: inconel 602ca, China inconel 602ca suppliers, inconel alloy radar system parts, B564 Uns N06625 Material Pipe, inconel alloy spinning process, inconel alloy nipple fittings, inconel alloy camshaft parts, inconel alloy shaft parts
Previous
Inconel 603XLYou Might Also Like
Send Inquiry