Incoloy Alloy 832 Seamless Pipe
video

Incoloy Alloy 832 Seamless Pipe

INCOLOY alloy 832 is an inexpensive stainless steel that can replace INCOLOY alloys 800 or 840 with specific addition of chemical elements that ensure formation of a protective and aesthetically pleasing surface oxide film. It exhibits excellent thermal stability and good resistance to pitting and hot salt corrosion. It is readily formed and has excellent weldability, which makes it suitable for use in.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 832 seamless pipe in China. If you're going to wholesale high quality incoloy alloy 832 seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ncoloy Alloy 832 is a nickel-chromium-iron alloy that also contains significant amounts of molybdenum, titanium, and aluminum. This alloy is particularly known for its excellent corrosion resistance in a wide range of environments, including stress corrosion cracking (SCC) in chloride-containing media and oxidizing acids. Incoloy Alloy 832 seamless pipe is fabricated through a process that ensures there are no seams or welds, which can be points of weakness in the pipe structure.

The chemical composition INCOLOY alloy 832 is outlined in the following table.

Element Content (%)
Iron, Fe 60.645 - 70.7
Chromium, Cr 19.5 - 21
Nickel, Ni 8.75 - 15.5
Copper, Cu ≤ 0.75
Silicon, Si 0.7
Titanium, Ti 0.4
Molybdenum, Mo 0.4
Manganese, Mn 0.4
Aluminum, Al 0.15
Carbon, C ≤ 0.050
Sulfur, S ≤ 0.0050

Physical Properties

The following table shows the physical properties of INCOLOY alloy 832.

Properties Metric Imperial
Density 7.75 g/cm3 0.280 lb/in3
Melting point 1450-1510°C 2642-2750°F

 

Incoloy Alloy 832 seamless pipeIncoloy Alloy 832 seamless pipeIncoloy Alloy 832 seamless pipe

Hot Tags: incoloy alloy 832 seamless pipe, China incoloy alloy 832 seamless pipe suppliers, Lncoloy 800H, alloy for tools, incoloy material pipe alloy, alloy for nitridation resistance, Inconel 825 Round Bar, precision alloy rod

Send Inquiry

whatsapp

Phone

E-mail

Inquiry