Gh4169 bushed hollow pipe
Chrome: 17.00-21.00
Molybdenum: 2.80 -3.30
Columbium + Tantalum: 4.75 -5.50
Titanium: 0.65 -1.15 Aluminum: 0.20 -0.80
Cobalt: 1.00 max Carbon: 0.80 max
Manganese: 0.35 max Silicon: 0.35 max
Phosphorus: 0.015 max Sulfur: 0.015 max
Boron: 0.006 maximum Copper: 0.30 maximum Iron: Balance
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh4169 bushed hollow pipe in China. If you're going to wholesale high quality gh4169 bushed hollow pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Gh4169 bushed hollow pipe introduce
Gh4169 alloy pipe


GH4169 alloy is a nickel-based high-temperature alloy precipitated and strengthened by body-centered square γ" and face-centered cubic γ' phases. It has good comprehensive properties in the temperature range of -253~700°C, and the yield strength below 650°C ranks among the highest deformation temperatures. It ranks first among alloys and has good fatigue resistance, radiation resistance, oxidation resistance, corrosion resistance, as well as good processing performance, welding performance and long-term structural stability. It can manufacture various parts with complex shapes and is used in aerospace, nuclear energy, In the petroleum industry, it has been widely used in the above temperature range. Another feature of this alloy is that the alloy structure is particularly sensitive to the thermal processing process. It is necessary to master the phase precipitation and dissolution rules in the alloy and the relationship between the structure, process, and properties. , reasonable and feasible process procedures can be formulated according to different use requirements, and various parts that can meet different strength levels and use requirements can be obtained. The varieties supplied include forgings, forged bars, rolled bars, cold-rolled bars, round cakes, Rings, plates, belts, wires, tubes, etc. It can be made into disks, rings, blades, shafts, fasteners and elastic elements, plate structural parts, casings and other parts for long-term use in aviation.
Gh4169 bushed hollow pipe
|
Element |
C |
Cr |
Ni |
Co |
Mo |
Al |
Ti |
Fe |
|
Weight(%) |
0.08 max |
17.00~21.00 |
50.00~55.00 |
1.00 max |
2.80~3.30 |
0.20~0.80 |
0.65~1.15 |
Rem |
|
Element |
Nb |
B |
Mg |
Mn |
Si |
P |
S |
Cu |
|
Weight(%) |
4.75~5.50 |
0.006 max |
0.010 max |
0.35 max |
0.35 max |
0.015 max |
0.015 max |
0.300 max |
Equivalent grade of GH4169
| China | GB | GH4169 (GH169) |
| ISC | H41690 | |
| USA | Commercial grade | Inconel 718 |
| UNS | N07718 | |
| SAE | XEV-1 | |
| AMS | 5596 5662 |
|
| Germany | DIN EN/DIN | NiCr19NbMo |
| W-Nr. | 2.4668 | |
| France | NF EN/NF | ATG C1 NC19FeNb |
| UK | Commercial grade | Inconel 718 |
Application of GH4169 high temperature alloy
Gh4169 pipe

GH4169 high temperature alloy has the characteristics of high strength, good toughness, good corrosion resistance, high high temperature stability, etc., and is widely used in aviation, aerospace, petroleum, chemical industry and other fields. In the field of aerospace, GH4169 is mainly used to manufacture high temperature parts, such as turbine blades, turbine discs, combustion chambers, etc. In the field of petrochemicals, GH4169 is often used to manufacture reactors, steam generators, hydrogenation equipment, etc. In addition, GH4169 can also be used to manufacture automobile emission systems, nuclear power plant reactors and other fields.
GNEE Group Factory Environment
Gh4169 high temperature alloy

GNEE Group Product Packaging
Gh4169 high temperature alloy pipe

FAQ
Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.
Hot Tags: Gh4169 bushed hollow pipe, China Gh4169 bushed hollow pipe suppliers, construction alloy, Monel N04400 N05500 Thick Wall Pipe, tool alloy, equipment alloy, product alloy, turbine alloy
You Might Also Like
Send Inquiry