Hastelloy B2 Alloy Round Forged Bar
Length: 0.5 - 6.0 meter
Diameter: 3 - 600 mm
Surface: Pickled, Black, Bright,Polished
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy b2 alloy round forged bar in China. If you're going to wholesale high quality hastelloy b2 alloy round forged bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy B2 Alloy Round Bar introduce
Hastelloy B2 Alloy Forged Bar


Hastelloy B2 round bars have resisted imperious use of oxygen-filled climates; it is not subsequently proposed as a result of an adverse erosion debacle in oxidation media or in engaging in cupric and ferrous sales. Hastelloy B2 round baris a solid nickel-molybdenum alloy, strengthened solution, with significant resistance to reduction, e.g. in gas and sulfuric, acetic and phosphoric acid conditions. The solution provides significant resistance.
Hastelloy B2 round bar specifications
Specifications: ASTM B335 / ASME SB335
Size: 5mm to 500mm
Diameter: 0.1mm to 100mm
Length: 100mm to 3000mm and above
Shape: round, square, hexagonal (A/F), rectangular, etc.
Surface treatment: black, bright polished, rough turned, NO.4 surface treatment, matte surface treatment, BA surface treatment
Hastelloy Alloy B2 Round Bar Chemical Composition
| Grade | Ni | Mo | Fe | C | Co | Cr | Mn | Si | P | S |
| Alloy B2 | Balance | 26.0-30.0 | 2.0 max | 0.02 max | 1.0 max | 1.0 max | 1.0 max | 0.10 max | 0.040 max | 0.030 max |
Nickel Alloy B2 Round Bar Mechanical Properties
| Element | Density | Melting Point | Tensile Strengt | Yield Strength (0.2%Offset) | Elongation |
| Alloy B2 | 9.2 g/cm3 | 1370 °C (2500 ºF ) | Psi – 1,10,000, MPa – 760 | Psi – 51000, MPa – 350 | 40 % |
GNEE Group Factory Environment
B2 Alloy Round Forged Bar

GNEE Group Product Packaging
Hastelloy metal B2 Alloy Round Forged Bar

GNEE Group Product Testing
Hastelloy B2 metal Round Forged Bar

FAQ
Q: What is your terms of payment?
A: 20% Prepayment and balance see B/L copy or 100%LC at sight.
Q: Are you a factory or a trading company?
A: We are a professional manufacturer, and our company is also a very professional steel products trading company. We can offer a wide range of steel as well as super stainless steel products.
Q: What does your factory do in terms of quality control?
A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.
Hot Tags: Hastelloy B2 Alloy Round Forged Bar, China Hastelloy B2 Alloy Round Forged Bar suppliers, alloy stainless pipe, high nickel corrosion alloys, inconel piping, alloy inconel tube, nickel based alloy, Duplex Stainless Steel
You Might Also Like
Send Inquiry