Hastelloy B2 Alloy Round Profile Rod

Hastelloy B2 round bar specifications
Size: 5 mm to 500 mm
Diameter: 0.1 mm to 100 mm
Length: 100 mm to 3000 mm and above
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy b2 alloy round profile rod in China. If you're going to wholesale high quality hastelloy b2 alloy round profile rod made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy B2 Alloy Profile Rod introduce

Hastelloy B2 Alloy Round Rod

Hastelloy B2 Alloy Round Profile RodHastelloy B2 Alloy Round Profile Rod

Hastelloy B2 rods are a nickel–the base made of hydrochloric acid is an excellent resistance at all temperatures and concentrations. Hastelloy B2 rodsare extremely resistant to any hydrochloric acid temperature and concentration. Hastelloy B2 rodswere made from the nickel alloy' as produced' molybdenum. Hastelloy B2 rodis a solid reinforced molybdenum nickel alloy that is typically used in conditions that are very reduced.

B2 Alloy Round Bar is a nickel-molybdenum alloy that is resistant to pitting and stress corrosion cracking. It is ideal for applications requiring high chemical corrosion resistance. This bar has proven to perform well in extremely corrosive applications such as chemical processing, waste treatment and petrochemical.

Hastelloy B2 Round Bar Specifications
Specifications : ASTM B335 / ASTM SB335
Dimensions : EN, DIN, JIS, ASTM, BS, ASME, AISI
Size : 5 mm To 500 mm
Diameter : 0.1 mm to 100 mm
Length : 100 mm To 3000 mm Long & Above
Finish : Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish
Tolerance : H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients' requirements
Form : Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc.

Chemical Properties of Hastelloy B2 Round Bar

Grade Ni Mo Cr Fe Mn C P S Si
Hastelloy B2 Bal 26 - 30 1.0 - 0.1 0.02 0.04 0.03 0.1

GNEE Group Product Testing

Hastelloy B2 Round Profile Rod

Hastelloy B2 Alloy Round Profile Rod

GNEE Group Factory Environment

B2 Alloy Round Profile Rod

Hastelloy B2 Alloy Round Profile Rod

FAQ

Q: What is your terms of payment?
A: 20% Prepayment and balance see B/L copy or 100%LC at sight.
Q: Are you a factory or a trading company?
A: We are a professional manufacturer, and our company is also a very professional steel products trading company. We can offer a wide range of steel as well as super stainless steel products.
Q: What does your factory do in terms of quality control?
A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality. 

Hot Tags: Hastelloy B2 Alloy Round Profile Rod, China Hastelloy B2 Alloy Round Profile Rod suppliers, piping seamless stainless steel, alloy for forging, alloy for marine applications, hastelloy material, alloy for batteries, Hastelloy B2

Send Inquiry

whatsapp

Phone

E-mail

Inquiry