SS 430 Bright Treated Stainless Steel Finish Coils
video

SS 430 Bright Treated Stainless Steel Finish Coils

SS 430 Bright treated (BA)finish coils created by heat-treating (annealing) steel with a controlled atmosphere chamber. After heat-treatment, the steel encompasses a reflective, mirror-like look, however may additionally have some imperfections and cloudiness.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss 430 bright treated stainless steel finish coils in China. If you're going to wholesale high quality ss 430 bright treated stainless steel finish coils made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SS 430 Bright treated (BA)finish coils created by heat-treating (annealing) steel with a controlled atmosphere chamber. After heat-treatment, the steel encompasses a reflective, mirror-like look, however may additionally have some imperfections and cloudiness.

SS 430 Bright treated (BA)finish coils one kind of common steel with good corrosion resistance, better thermal conductivity than austenitic, smaller Coefficient of thermal expansion than austenite, heat resistant etc

4 110 -

 

Grades SS 430
Tensile Strength (MPa) min 450
Yield Strength 0.2% Proof (MPa) min 205
Elongation (% in 50mm) min 22
Hardness Rockwell B (HR B) max 89
Hardness Brinell (HB) max 183