Monel K-500 Square Bar
video

Monel K-500 Square Bar

MONEL® alloy K-500 (UNS N05500 / W.Nr. 2.4375) is a nickel-copper alloy which combines the excellent corrosion resistance of MONEL alloy 400 with the added advantages of greater strength and hardness. The increased properties are obtained by adding aluminum and titanium to the nickel-copper base.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel k-500 square bar in China. If you're going to wholesale high quality monel k-500 square bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel K-500 Square Bar

Product Introduction

Monel K-500 square bar is nickel alloy bars with square section. Depending on the manufacturing process and size, Monel K-500 square bars can be hot-rolled from Monel K-500 billet or cold-drawn from Monel K-500 round bar & rod. We provide Monel K-500 square bars with polished, pickled and sandblasted finish for your choice.

Data Sheet

Physical Properties

Density g/cm3 8.44
lb/in.3 0.305
Melting Range °F 2400 - 2460
°C 1315 - 1350

Mechanical Properties

Condition & Size Tensile Strength Yield Strength
(0.2% Offset)
Elongation Reduction of Area Hardness
MPa, min MPa, min %, min %, min Rockwell C, min
Hot-worked and age-hardened /
All sizes
140 (965) 100 (690) 20.0 ... 27
Annealed and age-hardened /
Up to 1 (25.4)
130 (895) 90 (620) 20.0 ... 24
Annealed and age-hardened /
1 (25.4) and over
130 (895) 85 (585) 20.0 ... 24

monel k500 bar

monel square bar