Is Inconel a nickel-based alloy?

Is Inconel a nickel-based alloy?

 

 

Inconel is a nickel-chromium-based superalloy often utilized in extreme environments where components are subjected to high temperature, pressure or mechanical loads. Inconel alloys are oxidation- and corrosion-resistant. When heated, Inconel forms a thick, stable, passivating oxide layer protecting the surface from further attack. Inconel retains strength over a wide temperature range, attractive for high-temperature applications where aluminum and steel would succumb to creep as a result of thermally-induced crystal vacancies. Inconel's high-temperature strength is developed by solid solution strengthening or precipitation hardening, depending on the alloy.

Is Inconel a nickel-based alloy?Is Inconel a nickel-based alloy?

Inconel alloys are typically used in high temperature applications. Common trade names for various Inconel alloys include:

Alloy 625: Inconel 625, Chronin 625, Altemp 625, Sanicro 625, Haynes 625, Nickelvac 625 Nicrofer 6020 and UNS designation N06625.
Alloy 600: NA14, BS3076, 2.4816, NiCr15Fe (FR), NiCr15Fe (EU), NiCr15Fe8 (DE) and UNS designation N06600.
Alloy 718: Nicrofer 5219, Superimphy 718, Haynes 718, Pyromet 718, Supermet 718, Udimet 718 and UNS designation N07718.

Specific data

Alloy Solidus °C (°F) Liquidus °C (°F)
Inconel 600 1354 (2,469) 1413 (2,575)
Inconel 617 1332 (2,430) 1377 (2,511)
Inconel 625 1290 (2,350) 1350 (2,460)
Inconel 690 1343 (2,449) 1377 (2,511)
Inconel 718 1260 (2,300) 1336 (2,437)
Inconel X-750 1390 (2,530) 1430 (2,610)