Oct 23, 2025 Leave a message

ASTM B163 UNS N02200 Seamless pipes for heat exchangers

 
ASTM B163 UNS N02200 Seamless pipes for heat exchangers
 
ASTM B163 UNS N02200 Seamless pipes for heat exchangers

ASTM B163 UNS N02200 Seamless pipes for heat exchangers

ASTM B163 UNS N02200 seamless tubing, also known as Pure Nickel 200, is specified for heat exchangers and condensers due to its excellent corrosion resistance, high-temperature strength, and mechanical properties. Key features include consistent chemical composition and mechanical properties (such as tensile and yield strength), a wide range of sizes, and extensive testing requirements to ensure performance. It is suitable for a wide range of applications involving reducing acids and generally high-temperature environments.

What is SB 163 tubing?

SB 163 specifies nickel and nickel alloy seamless tubing for use in condensers and heat exchangers. These tubing is constructed from various alloy grades, such as Alloy 400, Alloy 600, Alloy 800, and Nickel Alloy 200/201. These materials are selected for their ability to withstand high temperatures and severe corrosive environments.

SB 163 Tubing
 

ASTM B163 UNS N02200 is the specification for seamless nickel and nickel alloy condenser and heat exchanger tubing. UNS N02200 represents commercially pure nickel (99.6%) and is commonly used in a variety of industrial applications due to its excellent corrosion resistance and high thermal conductivity. ASTM B163 outlines the chemical composition, mechanical properties, dimensions, and tolerance requirements for UNS N02200 and other nickel alloy seamless tubing.

 

Chemical Composition of ASTM B163 UNS N02200

Grade   Cu Iron Mn C Si Ni S
N02200 Min           99.0  
Max 0.25 0.40 0.35 0.15 0.35   0.01

 

Mechanical Properies of ASTM B163 UNS N02200

Grade Tensile Str Ksi(Mpa) Yield Str Ksi(Mpa) Elongation(%) Rockwell C(HRC)
N02200 ≥55(379) ≥15(103) ≥40 ≥65

 

Material Properties
Alloy: UNS N02200 is high-purity nickel.
Corrosion Resistance: Excellent resistance to a variety of corrosive environments, especially reducing acids.
Mechanical Properties: Meets specified tensile strength, yield strength, and elongation requirements, depending on the condition (e.g., annealed or stress-relieved).
High-Temperature Performance: Retains strength at high temperatures, making it suitable for heat exchange applications.

 

Specifications and Testing
Standard: ASTM B163 covers seamless tubing for condensers and heat exchangers.
Chemical Composition: Must meet specified limits for elements such as nickel and carbon.
Testing: Includes mechanical tests such as tensile strength and hardness, as well as chemical analysis and other tests such as grain size and flattening.
Marking: Tubes are marked with heat number, thickness, outside diameter, grade, and standard lengths.

 

Applications
Heat Exchangers: Due to its thermal conductivity and corrosion resistance, it is widely used for heat exchange in a variety of industries.
Condensers: Suitable for condenser applications.
Chemical Processing: Used in applications exposed to reducing, acidic solutions.
Furnace and Aerospace: Used in high-temperature environments and the aerospace industry.

 

Sizes and Shapes
Shapes: Seamless pipe and tube.
Sizes: Available in a variety of sizes, typically expressed in terms of outside diameter (OD) and wall thickness (WT).
Thickness: Wall thickness ranges from 1.24 mm to 40.49 mm (0.049 in. to 1.594 in.).
Outer Diameter: Ranges from 10.3 mm (0.406 in.) to 426 mm (16.77 in.).
Limitations: This specification covers sizes up to 3 in. (76.2 mm) outside diameter, with certain wall thickness restrictions.

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production of various nickel-based alloys. Gnee Steel's product packaging includes steel strapping: Pipes with an outer diameter of 3 inches or less are typically strapped together with polypropylene film to prevent rust during sea transportation, and then secured with steel strapping. Wooden boxes/crates: Pipes are typically packaged in wooden boxes or crates to protect them during transportation, especially those that are longer or have larger diameters. Seaworthy export packaging: Suppliers typically use standard seaworthy export packaging methods, which may include a variety of materials and techniques to protect the pipes during transportation. Tarpaulin packaging: This prevents rain, seawater, and other external factors from penetrating the export wooden crates during transportation. Gnee Steel specializes in the production and sale of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power, automotive, and nuclear energy industries, and we can provide customized alloy material solutions based on customer needs. For alloy material pricing inquiries or customized alloy material solutions, please contact us for a quote at ss@gneesteel.com.