Inconel 601 Alloy Round Bar
video

Inconel 601 Alloy Round Bar

Inconel 601 round bar

Length: 0.5 - 6.0 m
Diameter: 3 - 600 mm
Surface: blackened, pickled, bright, polished

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 601 alloy round bar in China. If you're going to wholesale high quality inconel 601 alloy round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

 

Ni 601 Alloy Round Bar Description

Inconel 601 Alloy Round Bar

 

Gnee Steel Inconel 601 Alloy Round Bar

Gnee Steel offers Inconel 601 Round Bars, also known as Nickel Alloy 601 Bars. These round bars have a nickel content of 58-63%. Inconel 601 is a general purpose nickel-chromium-iron alloy. It is a popular engineering alloy, especially for applications that require heat and corrosion resistance. Most industries choose Inconel 601 Round Bars because of its unmatched quality. These round bars are mainly used in harsh service conditions. Inconel 601 Bars are known for its unbreakable strength under impact loads. Moreover, it can withstand high temperatures and resist stress and pitting cracking.

Size of INCONEL 601 ROUND BAR :

 

Size Chucked true to OD Chucked true to ID
OD,
mm
ID,
mm
Max. OD,
mm<
Min. ID,
mm
Max. OD,
in.
Min. ID,
in.
Max. OD,
mm
Min. ID,
mm
Max. OD,
in.
Min. ID,
in.
32 20 31 21.9 1.220 0.862 30 21 1.185 0.827
32 16 31 18 1.220 0.709 30 17 1.181 0.669
36 25 35 26.9 1.378 1.059 34.1 26 1.343 1.024
36 20 35 22 1.378 0.866 34 21 1.339 0.827
36 16 35 18.1 1.378 0.713 33.9 17 1.335 0.669
40 28 39 29.9 1.535 1.177 38.1 29 1.500 1.142
40 25 39 27 1.535 1.063 38 26 1.496 1.024
40 20 39 22.1 1.535 0.870 37.9 21 1.492 0.827
45 32 44 33.9 1.732 1.335 43.1 33 1.697 1.299
45 28 44 30 1.732 1.181 43 29 1.693 1.
45 20 44 22.2 1.732 0.874 42.8 21 1.685 0.827

 

601 Alloy Round Bar Specifications

Chemical Composition of Alloy 601 Round Bars

Inconel 601 Ni Fe C Mn Si Cu Cr S Al
58.0 – 63.0 Balance 0.10 max 1.0 max 0.5 max 1.0 max 21.0 – 25.0 0.015 max 1.0 – 1.7

Mechanical Properties of Inconel 601 Bars

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 601 8.1 g/cm3 1411 °C (2571 °F) Psi – 80,000 , MPa – 550 Psi – 30,000 , MPa – 205 30 %

601 Alloy Bar Testing And Qualification Certificate

Inconel 601 Round Bar Testing And Qualification Certificate

Inconel 601 Round Bar Testing

Inconel 601 Round Bar Testing

Inconel 601 Round Bar Testing And Qualification Certificate
Inconel 601 Round Bar Qualification Certificate

About Gnee Steel

Gnee Steel

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 601 Round Bar, covering tubes: Seamless tubes: Size: 4 - 219 mm; Thickness: 0.5 - 20 mm; Welded tubes: Size: 5.0 - 1219.2 mm; Thickness: 0.5 - 20 mm, Plates: Plate thickness 0.1 to 100 mm; Plate width 10-2500 mm, Strips, Alloy Round Bar Sizes: Diameter 3-800 mm;, Flat Bar Sizes: Thickness 2-100 mm; Width: 10-500 mm, Hexagonal Bar Sizes: 2-100 mm;, Wire and Extruded Profiles. We work with steel mills to provide customers with 625 alloy that meets or exceeds many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Inconel 601 Round Bar, Tube, Pipe, Plate, Strip, Plate, Round Bar, Flat Bar, Forged Billet, Hexagon, Wire and Extruded Profiles. Feel free to contact us for a quote at ss@gneesteel.com

Hot Tags: inconel 601 alloy round bar, China inconel 601 alloy round bar suppliers, inconel alloy actuator parts, inconel alloy intake system parts, Inconel 617 Super Stainless Pipe, Inconel 693 Alloy Piping, alloy pipe, inconel alloy cylinder parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry