AMS 5540 Inconel 600 UNS N06600 Aerospace Annealed Sheet
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ams 5540 inconel 600 uns n06600 aerospace annealed sheet in China. If you're going to wholesale high quality ams 5540 inconel 600 uns n06600 aerospace annealed sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
AMS 5540 Inconel 600 UNS N06600 aerospace annealed sheet is a nickel‑chromium‑iron alloy plate produced to aerospace‑grade specifications. It is supplied in the annealed condition to deliver balanced ductility and stable mechanical properties. This alloy resists high‑temperature oxidation and stress corrosion cracking, maintaining reliable performance under cyclic thermal loads.
It undergoes strict PMI, dimensional inspection and surface examination to satisfy aerospace traceability and acceptance rules. Typical uses include aircraft exhaust components, heating ducts and engine auxiliary structures, where consistent metallurgy and forming capability are required for high‑temperature service.




Chemical Composition of AMS 5540 Nickel 600
This chemical range complies strictly with AMS 5540 aerospace specification for annealed Inconel 600 sheet. Every batch is verified by PMI test to eliminate material mixing and meet aerospace traceability requirements.
| Element | Content (wt.%) |
|---|---|
| Ni (Nickel) | ≥72.0 |
| Cr (Chromium) | 14.0 – 17.0 |
| Fe (Iron) | 6.0 – 10.0 |
| C (Carbon) | ≤0.15 |
| Mn (Manganese) | ≤1.00 |
| Si (Silicon) | ≤0.50 |
| S (Sulfur) | ≤0.015 |
| Cu (Copper) | ≤0.50 |
Mechanical Properties of AMS 5540 Inconel 600
These mechanical limits apply to annealed AMS 5540 Inconel 600 aerospace sheet. Each heat lot is sampled and tested to confirm compliance, supporting forming and high‑temperature service for aviation components.
| Property | Requirement |
|---|---|
| Tensile Strength, Rm | 550 MPa (80 ksi) min |
| Yield Strength, Rp0.2 | 240 MPa (35 ksi) min |
| Elongation (50 mm / 2 in gauge) | 30 % min |
| Hardness, HB | ≤187 HB |
Note: Room temperature, longitudinal direction; values represent minimum requirements
Heat Treatment Properties of Inconel 600 Aerospace sheet (AMS 5540)
Applicable to annealed UNS N06600 sheet for aerospace service
| Item | Details |
|---|---|
| Standard delivery condition | Full annealed, the required state for AMS 5540 aerospace sheet |
| Annealing temperature range | 980 ℃ – 1040 ℃, hold for proper soaking time |
| Cooling method | Air cool or water quench to retain uniform austenitic grain structure |
| Core function of annealing | Dissolve carbide precipitates, reduce residual stress, maximize ductility for forming |
| Age hardening response | Non-age-hardenable; strength cannot be improved by aging treatment |
| Stress relief treatment | 870–900 ℃, slow cooling, used after bending, stamping or forming operations |
| Grain structure after full anneal | Uniform equiaxed austenite, stable under cyclic high-temperature exposure |
AMS 5540 specifies full annealed supply condition. Avoid overheating above 1040 ℃ to prevent excessive grain coarsening, which reduces ductility and fatigue resistance for aerospace parts.
Surface Finishing Process for UNS N06600 Aerospace sheet
| Item | Details |
|---|---|
| Pickling & passivation | Acid pickling removes oxide scale after heat treatment; passivation forms stable Cr₂O₃ film |
| Bright annealing | In protective atmosphere, oxide-free bright surface, no subsequent pickling required |
| Sand blasting | Fine glass bead blasting, uniform matte surface, removes surface defects |
| Polishing | Mechanical polishing to Ra 0.4–1.6 μm, for high-purity / nuclear heat exchanger tubing |
AMS 5540 Aerospace Annealed Sheet Tolerances
Note: SAE AMS 5540 references AS4194 for dimensional tolerances, for UNS N06600 Inconel 600 annealed aerospace sheet, max nominal thickness 50.8 mm (2 in)
| Tolerance Item | Nominal Size Range | Permissible Tolerance |
|---|---|---|
| Sheet Thickness | ≤ 0.40 mm | ±0.03 mm |
| Sheet Thickness | >0.40 ~ 1.60 mm | ±0.05 mm |
| Sheet Thickness | >1.60 ~ 6.35 mm | ±0.08 mm |
| Sheet Thickness | >6.35 ~ 50.80 mm | ±0.13 mm |
| Width | ≤ 1220 mm | 0 / +1.6 mm |
| Width | >1220 mm | 0 / +3.2 mm |
| Length | ≤ 2440 mm | 0 / +3.2 mm |
| Length | >2440 mm | 0 / +6.4 mm |
| Flatness | All sheet gauges | Max 6 mm deviation per 1000 mm span |
| Edge Cut | Sheared / machined edge | ±0.8 mm |
AMS 5540 itself does not fully list all dimensional limits; tolerance rules follow AS4194 aerospace flat product specification. All sheets are inspected dimensionally before release to satisfy aerospace traceability requirements.
Advantages of Inconel 600 for Aerospace
High-Temperature Oxidation Resistance
It maintains a continuous protective Cr₂O₃ oxide layer up to 600 ℃, with oxidation rate below 0.1 mm per 1000 h, resisting scaling for exhaust ducts and heating components.
Stable Mechanical Performance at Elevated Temperature
At 538 ℃, the alloy retains minimum tensile strength of 480 MPa. Its annealed structure avoids rapid strength drop under cyclic thermal load in airborne service.
Stress Corrosion Cracking Resistance
In chloride and humid high-temperature environments, it shows far lower crack growth rate than 321 stainless steel, reducing failure risk for pressurized aerospace auxiliary structures.
Excellent Formability for Complex Parts
Annealed AMS 5540 sheet delivers minimum 30% elongation. It supports deep drawing and bending without cracking to fabricate irregular aircraft thermal components.
Typical Applications of Alloy 600 Aerospace sheet

Aircraft Exhaust System Components
Aircraft Heating & Environmental Ducting


Auxiliary Engine Thermal Shield Parts
Aerospace Ground Support Thermal Hardware
Applied to high-temperature test fixtures and heating chambers. It maintains stable grain structure after hundreds of heating cycles for repeated aerospace component qualification tests.

Why Choose GNEE STEEL as Your Supplier of Nickel Alloy Seamless Tubes?
Standard compliance:
Our nickel alloy seamless tubes comply with ASME B167, RCC-M and other applicable nuclear-grade specifications. Each batch is produced, inspected and documented following the designated code requirements to satisfy nuclear project qualification rules.
Tight chemical control:
We implement strict melting and analysis control for chemical composition. Trace impurities and cobalt content are limited to ultra-low levels, which reduces activation risk and meets nuclear radiation service requirements.
Full non-destructive testing:
Every tube undergoes 100% eddy current testing plus ultrasonic inspection. The acceptance threshold for internal and surface defects is set to stringent nuclear-grade limits to avoid hidden service failures.
Individual hydrostatic test:
Each seamless tube is subjected to a separate hydrostatic test at the specified pressure. We record test pressure, holding time and visual check results to verify reliable pressure-bearing performance.




Get MTC for Nickel 600 seamless tube/pipe
Packaging and Shipping


Hot Tags: ams 5540 inconel 600 uns n06600 aerospace annealed sheet, China ams 5540 inconel 600 uns n06600 aerospace annealed sheet suppliers, Inconel 600 Plate, inconel alloy cooling system parts, inconel alloy extrusion molding process, inconel alloy piston parts, inconel alloy resistor parts, Inconel UNS N06625 Pipe