ASME Sb514 Incoloy 800h Weld Tube Nickel-Iron-Chromium Alloy Steel
ASME SB 514 N08800 welded pipe: OD: 6-200mm, wall thickness: 0.35-6.00mm
European and American standards:
ASTM B514, ASME SB 514, UNS N08800, WNR 1.4876, ISO 6207, VdTüV 412 and 434, BS3 3074NA15, DIN 17459
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of asme sb514 incoloy 800h weld tube nickel-iron-chromium alloy steel in China. If you're going to wholesale high quality asme sb514 incoloy 800h weld tube nickel-iron-chromium alloy steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASME Sb514 Incoloy 800h Weld Tube Alloy Steel
ASME Sb514 800h Weld Tube Nickel-Iron-Chromium Alloy Steel


| Standard: | ASME SB514 | Certification: | ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008 |
|---|---|---|---|
| Test: | ET, UT, HT, PT | Type: | Seamless, Welded |
| O.D.: | 1- 254 Mm | W.T.: | 0.1 To 20mm |
| High Light: |
nickel-iron-chromium alloys Weld Tube,Incoloy 800H Weld Tube,ASME SB514 Weld Tube |
||
What is ASME SB514 Incoloy 800H Weld Tube ?
ASME SB514 is a specification published by the American Society of Mechanical Engineers (ASME) that covers the requirements for seamless and welded tubes made of Incoloy 800H alloy. Incoloy 800H is a nickel-iron-chromium alloy with high strength and excellent resistance to oxidation, carburization, and nitridation. It is commonly used in high-temperature applications such as heat exchangers, furnace components, and petrochemical processing equipment.
The ASME SB514 specification provides guidelines for the dimensions, mechanical properties, and testing requirements of Incoloy 800H weld tubes. It specifies the allowable tolerances for outside diameter, wall thickness, and length of the tubes. The mechanical properties, such as tensile strength, yield strength, and elongation, are also specified to ensure the quality and performance of the tubes.
Furthermore, the ASME SB514 specification outlines the various non-destructive testing methods, such as ultrasonic examination and eddy current examination, that should be conducted to detect any defects or imperfections in the welds. It also includes requirements for the heat treatment of the tubes to achieve the desired mechanical properties.
ASME SB514 provides the necessary guidelines and requirements for the manufacturing and testing of Incoloy 800H weld tubes, ensuring their suitability for high-temperature applications.
EQUIVALENT GRADES FOR INCOLOY 800H WELDD TUBE
| STANDARD | WERKSTOFF NR. | UNS | JIS | EN | BS | GOST | AFNOR | OR |
| Incoloy 800H | 1.4958 | N08810 | NCF 800H | X5NiCrAlTi31-20 | NA 15(H) | ЭИ670 | Z8NC33-21 | XH32T |
ASTM B514 Incoloy 800H Pipe Chemical Composition
| Grade | C | Mn | Si | Fe | S | Cr | Al-Ti | Ni |
| minimum | 0.05 | - | - | 39.5 | - | 19.0 | 0.15 | 30.0 |
| maximum | 0.1 | 1.5 | 1.0 | - | 0.015 | 23.0 | 0.60 | 35.0 |
MECHANICAL PROPERTIES FOR INCOLOY 800H WELD TUBE
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.94 g/cm3 | 1385 °C (2525 °F) | Psi - 75,000 , MPa - 520 | Psi - 30,000 , MPa -205 | 30 % |
ASTM B514 Welded Pipes Specifications |
||
| Size | : | 6.00 mm OD up to 914.4 mm OD |
| Thickness | : | 0.3mm – 50 mm, SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS |
| Length | : | Within 13500mm |
| Type | : | Welded Pipes |
| Grades | : | UNS N08800, UNS N08810, UNS N08120 |
GNEE Group Factory Environment
Incoloy 800h Weld Tube

GNEE Group Product Packaging
Incoloy 800h Weld Tube Nickel-Iron-Chromium Alloy Steel

FAQ
Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, Russia, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.
Hot Tags: asme sb514 incoloy 800h weld tube nickel-iron-chromium alloy steel, China asme sb514 incoloy 800h weld tube nickel-iron-chromium alloy steel suppliers, welded alloy pipe, alloy for controllers, incoloy pipe alloy, alloy for sustainable development baths, alloy for generators, alloy for transformers