Alloy GH4169 Thick Walled SS Pipes
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy gh4169 thick walled ss pipes in China. If you're going to wholesale high quality alloy gh4169 thick walled ss pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Alloy GH4169 Thick Walled SS Pipes introduce
Alloy GH4169 Thick Walled SS Pipes


GH4169 Inconel 718 | UNS N007718 | NC19FENB | GH169
GH4169 alloy also known as Inconel 718 with a UNS designation of N007718. It is a nickel-based age-hardenable superalloy with a 650 °C service temperature. GH4169 has a high creep rupture strength, high tensile strength, and excellent relaxation resistance.
GNEE group manufactures GH4169 usually used in the aerospace industry, petroleum, nuclear industry, and more. Due to its high durability, this alloy is suitable for manufacturing rotor components, power drive shafts, aircraft engines, turbine disks, compressor blades, etc.
At GNEE group we deliver high-grade GH4169 forms for your applications. Whether you need GH4169 sheets, GH4169 plates, GH4169 rods, GH4169 bar, GH4169 coil, GH4169 strip, or GH4169 tubes, you can find high-performance products here at competitive pricing. All products have to comply with ISO, ASTM, JIS standards, etc. Standard and custom sizes are available depending on your specifications.
Chemical composition of GH4169 alloy(%)
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | 50.0 – 55.0 |
| Chromium (Cr) | 17.0 – 21.0 |
| Iron (Fe) | Balance |
| Molybdenum (Mo) | 2.8 – 3.3 |
| Niobium (Nb) + Tantalum (Ta) | 4.75 – 5.5 |
| Titanium (Ti) | 0.65 – 1.15 |
| Aluminum (Al) | 0.2 – 0.8 |
| Cobalt (Co) | ≤ 1.0 |
| Manganese (Mn) | ≤ 0.35 |
| Silicon (Si) | ≤ 0.35 |
| Sulfur (S) | ≤ 0.015 |
| Phosphorus (P) | ≤ 0.015 |
| Carbon (C) | ≤ 0.08 |
| Copper (Cu) | ≤ 0.3 |
| Boron (B) | 0.001 – 0.006 |
GH4169 - Form of Supply
| Product type | Products | Dimension | Processes | Deliver Status |
|---|---|---|---|---|
| Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
| Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |
Alloy GH4169 Thick Walled SS Pipes size and weight
| Dimensions | Wall | Weight per | Dimensions | Wall | Weight per | |
|---|---|---|---|---|---|---|
| (mm) | (mm) | metre (kg) | (mm) | (mm) | metre (kg) | |
| 12.7 x 12.7 | 1.20 | 0.44 | 40 x40 | 1.20 | 1.49 | |
| 12.7 x 12.7 | 1.50 | 0.55 | 40 x40 | 1.50 | 1.85 | |
| 15 x 15 | 1.20 | 0.53 | 40 x40 | 2.00 | 2.45 | |
| 15 x 15 | 1.50 | 0.65 | 40 x40 | 3.00 | 3.75 | |
| 20 x 20 | 1.20 | 0.71 | 50 x50 | 1.50 | 2.32 | |
| 20 x 20 | 1.50 | 0.88 | 50 x50 | 2.00 | 3.08 | |
| 20 x 20 | 2.00 | 1.19 | 50 x50 | 3.00 | 4.65 | |
| 25 x 25 | 1.20 | 0.92 | 60 x60 | 2.00 | 3.71 | |
| 25 x 25 | 1.50 | 1.14 | 60 x60 | 3.00 | 5.49 | |
| 25 x 25 | 2.00 | 1.49 | 70 x70 | 3.00 | 6.53 | |
| 25 x 25 | 3.00 | 2.20 | 80 x80 | 2.00 | 4.98 | |
| 30 x 30 | 1.20 | 1.10 | 80 x80 | 3.00 | 7.53 | |
| 30 x 30 | 1.50 | 1.37 | 100 x 100 | 2.00 | 6.40 | |
| 30 x 30 | 2.00 | 1.84 | 100 x 100 | 3.00 | 9.53 | |
| 30 x 30 | 3.00 | 2.72 | ||||
GNEE Group Factory Environment
Alloy GH4169 Thick Walled SS Pipes

GNEE Group Product Delivery
Thick wall 718 Inconel tube

FAQ
Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.
Hot Tags: Alloy GH4169 Thick Walled SS Pipes, China Alloy GH4169 Thick Walled SS Pipes suppliers, precision alloy, industrial alloy, construction alloy, engine alloy, Monel R405, aerospace alloy