Hastelloy C2000 BAR
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy c2000 bar in China. If you're going to wholesale high quality hastelloy c2000 bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
This alloy was developed to broaden the application range of one alloy. With the addition of Copper to the Nickel-Chromium-Molybdenum system, Hastelloy C-2000 is resistant to an extensive range of corrosive chemicals, including sulphuric, hydrochloric and hydrofluoric acids. The combination of Molybdenum and Copper provide excellent corrosion resistance to reducing media, while the high Chromium content gives good oxidising resistance.
Common Trade Names:
Hastelloy C2000 /UNS N06200 /NS3405 /AWS 055 /W.Nr 2.4675
Specifications:
ASTM B564, ASTM B574,ASTM B575,ASTM B619,ASTM B622, ASTM B366
Characteristic:
Developed to resist corrosion in a wider range of media.
Resistant to an extensive range of corrosive chemicals including sulphuric, hydrochloric & hydrofluoric acids.
Superior pitting resistance and crevice corrosion resistance to Hastelloy C-276.
Excellent corrosion resistance to reducing media.
Good oxidising resistanc
Hastelloy C2000 Chemical Composition
| % | Cr | Mo | Fe | C | Si | Co | Mn | P | S | Cu | Al | Ni |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Min | 22 | 15 | – | – | – | – | – | – | – | 1.3 | – | - |
| Max | 24 | 17 | 3 | 0.01 | 0.08 | 2 | 0.5 | 0.025 | 0.01 | 1.9 | 0.5 | bal |
Hastelloy C2000 Physical Properties
| Density | Melting Point | Coefficient of Expansion | Modulus of Rigidity | Modulus of Elasticity |
|---|---|---|---|---|
| 8.5 g/cm³ | 1399 °C | 12.4 μm/m °C (20 – 100 °C) | 79 kN/mm² | 206 kN/mm² |
| 0.307 lb/in³ | 2550 °F | 6.9 x 10-6 in/in °F (70 – 212 °F) | 11458 ksi | 29878 ksi |
Hastelloy C2000 Heat Treatment
| Condition as supplied by AWI | Type | Temperature | Time | Cooling |
|---|---|---|---|---|
| Annealed or Spring Temper | Stress Relieve | 400 – 450 °C (750 – 840 °F) | 2 Hr | Air |
Hastelloy C2000 Heat Treatment Of Finished Parts
| Annealed | ||
|---|---|---|
| Approx. tensile strength | <1000 N/mm² | <145 ksi |
| Approx. operating temperature depending on load** and environment | -200 to +400 °C | -330 to +750 °F |
| Spring Temper | ||
|---|---|---|
| Approx. tensile strength | 1300 – 1600 N/mm² | 189 – 232 ksi |
| Approx. operating temperature depending on load** and environment | -200 to +400 °C | -330 to +750 °F |
Hastelloy C2000 Mechanical Properties
| Annealed | ||
|---|---|---|
| Approx. tensile strength | <1000 N/mm² | <145 ksi |
| Approx. operating temperature depending on load** and environment | -200 to +400 °C | -330 to +750 °F |
| Spring Temper | ||
| Approx. tensile strength | 1300 – 1600 N/mm² | 189 – 232 ksi |
| Approx. operating temperature depending on load** and environment | -200 to +400 °C | -330 to +750 °F |
Hastelloy C2000 Available Shape
Hastelloy C2000 Size Range
»Round Bar & Square Bar & Hexagon Bar
● Diameter : φ8~φ300mm Length:10mm-6000mm
● Hot forging, Hot Rolling, Cold Drawing
● Bright Surface, Polished Surface, Black Surface
»Tube & Pipe:Seamless Tube& Welded Pipe
● Cold Drawing Seamless Pipe: φ1.0~φ220mm
● Hot Extrusion pipe: φ50~φ250mm
● Others : U Blend Tube and Elbow
»Hot Rolled Plate & Cold Rolled Sheet
● Cold Rolling Sheet Thickness: ≦2.0mm Width:≦1500m
● Hot rolling Plate Thickness: ≧4.0mm Width: ≦2500m
»Strip & Tape Ribbon
● Thickness: ≧ 0.01mm Width: 15mm-300mm
● Cold rolling BA Strip, Hard & Soft Condition
»Straight Length Wire & Spool Wire
● Welding Wire: φ 0.1mm~6.0mm Cut length Rod: φ1.0~φ8.0mm
● Package : 5-25kg/Spool or Box




Hastelloy C2000 ApplicationsI
The chemical process industry reactor,heat exchanger,columns,and the pipe.
The pharmaceutical industry reactor and dryer.
Flue gas desulfurization system
FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: hastelloy c2000 bar, China hastelloy c2000 bar suppliers, alloy for industrial equipment, seamless ss pipe, alloy for valves, hastelloy material, Hastelloy C, UNS N06455 N10629 Hastelloy Pipe
Previous
UNS N06002 PipeYou Might Also Like
Send Inquiry