Nickel Alloy Coil Nickel 200
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel alloy coil nickel 200 in China. If you're going to wholesale high quality nickel alloy coil nickel 200 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Nickel Alloy 200 Coils
Gneegroup is a major supplier, and exporter of Nickel 200 Coils, which are made from high-quality standard raw materials and built to national and international specifications. Alloy 200 Coils are wrought materials that have been reinforced. The limitations of these alloys are integrated into single dual chemistry with UNS N02200 Coils, resulting in a single alloy with the best qualities of each. These Nickel 200 Coils are available in a variety of bespoke shapes and sizes to meet the needs of our customers, all at competitive pricing.
Nickel 200 Coils have extremely tough qualities that allow them to withstand these circumstances without pitting, crevice corrosion or stress corrosion cracking. Nickel Alloy 200 Coil material is resistant to dry chlorine and hydrogen chloride, allowing it to be used at temperatures as high as 550°C. Mineral acid Ni 200 Foil resistance varies depending on temperature and concentration, with or without an aerated solution. Nickel 200 Coils suppliers in Mumbai recommend using the alloy in de-aerated acid since it has significantly superior corrosion resistance in de-aerated acids.

| Standard | ASTM B162 / ASME SB162 |
| Thickness | 0.2mm – 5.0mm |
| Width | 3.2mm – 1500mm |
| Length | AS PER CUSTOMER'S REQUIREMENT |
| Test Certificate | Yes |
| Coils Hardness | Half Hard, Quarter Hard, Soft, Hard, Spring Hard |
| Value Added Services | Cutting, Beveling, Polishing, Threading, Destructive, Non Destructive, Ultrasonic Testing |
| Form | Coil / Strip |

Quivalent Grades Of Nickel Alloy 200 Coils
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Nickel 200 | 2.4066 | N02200 | NW 2200 | NA 11 | НП-2 | N-100M | Ni 99.2 |
Chemical Composition Of Nickel Alloy 200 Coils
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Nickel 200 | 0.15 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
Nickel Alloy 200 Coils Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Nickel 200 | 8.9 g/cm3 | 1446 °C (2635 °F) | Psi – 67000 , MPa – 462 | Psi – 21500 , MPa – 148 | 45 % |