Fe .40% max Mn .35% max Si .35% max Cu .25% max C .15% max
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel 200 alloy pipe in China. If you're going to wholesale high quality nickel 200 alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Nickel 200 Alloy pipe

 

The chemical composition Nickel 200 alloy is outlined in the following table.

(Ni) Nickel1

99.0 min

(Fe) Iron

0.40 max

(Mn) Manganese

0.35 max

(Si) Silicon

0.35 max

(Cu) Copper

0.25 max

(C) Carbon

0.02 max

(S) Sulfur

0.01 max

 

Nickel 200 Alloy Application

 

Nickel Alloy 200 has many different industrial applications including:

Electronic Component

Electrical components

Heating element wire

Battery connections/terminals

Chemical processing

Aerospace parts

Food processing

Synthetic fiber processing

 

Nickel 200 Alloy Feature

 

Nickel 200 has the following key features:

Commercially pure nickel.

Resistant to various reducing chemicals and caustic alkalis.

Good magnetostrictive properties.

High electrical and thermal conductivity.

Good ductility and low work hardening rate.

Good solderability and weldability.

 