Weling series: ERNiCrMo-3,ERNiCrMo-4,ERNiCrMo-13,ERNiCrFe-3,ERNiCrFe-7,ERNiCr-3,ERNiCr-7,ERNiCu-7,ERNi-1, ER70S-6. Standard: Conforms to Certification AWS A5.14 ASME SFA A5.14 Size: 0.8MM / 1.0MM / 1.2MM / 1.6MM / 2.4MM / 3.2MM / 3.8MM / 4.0MM / 5.0MM Form: MIG(15kgs/spool), TIG(5kgs/box),Strip
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ernicr-3 nickel chromium alloy tig welding wire b in China. If you're going to wholesale high quality ernicr-3 nickel chromium alloy tig welding wire b made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Weling series:
ERNiCrMo-3,ERNiCrMo-4,ERNiCrMo-13,ERNiCrFe-3,ERNiCrFe-7,ERNiCr-3,ERNiCr-7,ERNiCu-7,ERNi-1, ER70S-6.

Standard: Conforms to Certification AWS A5.14 ASME SFA A5.14

Size: 0.8MM / 1.0MM / 1.2MM / 1.6MM / 2.4MM / 3.2MM / 3.8MM / 4.0MM / 5.0MM

Form: MIG(15kgs/spool), TIG(5kgs/box),Strip

QQ20231019151005

Product Model
Standard
Application
ERNi-1
GB/T 15620: SNi2061
AWS 5.14: ERNi-1
Mainly used for welding industrial pure nickel.
ERNiCu-7
GB/T 15620: ERNi4060
AWS A5.14: ERNiCu-7
Mainly used for welding alloy such as ASTM B127,B163,B164,B165 etc.
ERNiCr-3
GB/T 15620: SNi6082
AWS A5.14: ERNiCr-3
Maily used for welding nickel base alloy and dissimilar steel.
ERNiCrMo-3
GB/T 15620: SNi6625
AWS A5.14: ERNiCrMo-3
Maily used for welding nickel base alloy and dissimilar steel.
ERNiCrMo-4
GB/T 15620: SNi6276
AWS A5.14: ERNiCrMo-4
Mainly used for welding HASTELLOY C-276 and other nickel base alloy.Also used for surfacing welding on the surfaces of carbon
steel.
ERCuNi
GB/T 9460: SCu7158
AWS A5.7: ERCuNi
Mainly used of welding 70-30 Cu-Ni alloys,composite metal made by 70-30 Cu-Ni alloys and 645- steel,composite metal of lining
structures based on 645- steel. Also used as cladding of 70-30 Cu-Ni alloys.

20231027152515

 

Q1. What are your company's main products

A1: Our main products are alloy materials, stainless steel, carbon steel, galvanized steel, aluminium products, etc.

Q2. How do you control quality ?

A2: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS Verified.