440A 440B 440C Stainless Steel Flat Bar Stock High Hardness
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 440a 440b 440c stainless steel flat bar stock high hardness in China. If you're going to wholesale high quality 440a 440b 440c stainless steel flat bar stock high hardness made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
440A 440B 440C Stainless Steel Flat Bar Stock High Hardness
Description
| Commodity:: | 440 Stainless Steel Flat Bar | Standard: | ASTM, AISI, DIN, JIS |
|---|---|---|---|
| Width: | 30-300 | Thickness: | 10-500mm |
| Length: | 1000-6000mm | Edge: | Slit Edge Mill Edge |
| Technique: | Cold Drawn Hot Rolled | Application: | Chemical Industrial |
| High Light: |
440A 440c stainless steel flat bar,440B 440c stainless steel flat bar,Martensitic 440c stainless steel flat stock |
||
High Hardness 440A 440B 440C Stainless Steel Flat / Martensitic Stainless Steel Grade 440C
| Products | Stainess Steel Flat Bar |
| Grade |
440A 440B 440C |
| Standard | ASTM GB EN JIS |
| Thickness | 4.0 - 100mm |
| Width | 20 - 400mm customs as request |
| Surface Finishing | Pickling , Hairline , Polished |
| Servie | Cutting , Heat treatment |
| Other Grade |
200 Series:201 202 300 Series: 301 304 304L 304H 309S 310S 314 316L 316Ti 317L 321 347 400 Series: 409L 410 420 430 431 436L 439 441 443 444 440A/B/C Others: S31803 S32750 904L 254SMO 253MA C276 Monel400 Inconel 600/625 |
| Application | Structure , Decoration , household, furniture , decoration,Mechanical processing |
| Other Products | Stainless Steel Plate / Sheet / Pipe / Bars / Strips.etc |
About 440 Stainless Steel
Type 440 Stainless Steel, as known as "razor blade steel," is a hardenable high-carbon chromium steel. When put under heat treatment it attains the highest hardness levels of any grade of stainless steel. Type 440 Stainless Steel, which comes in four different grades, 440A, 440B, 440C, 440F, offers good corrosion resistance along with abrasion resistance. All grades can be easily machined in their annealed state, they also offer resistance to mild acids, alkalis, foods, fresh water, and air. Type 440 can be hardened to Rockwell 58 harness.
Type 440 Stainless Steel Applications
Thanks to each grades outstanding properties, all grades of Type 440 Stainless Steel can be found in a number of different products including:
Pivot pins
Dental and surgical instruments
High quality knife blades
Valve seats
Nozzles
Oil pumps
Rolling element bearings
Type 440 Stainless Steel Chemical Composition
Each grade of Type 440 Stainless Steel is made up of a unique chemical composition. It should be noted that the only major difference between the grades is the level of Carbon
Type 440A
Cr 16-18%
Mn 1%
Si 1%
Mo 0.75%
P 0.04%
S 0.03%
C 0.6-0.75%
Type 440B
C 0.75-0.95%
Type 440C and 440F
C 0.95-1.20%
All of the Type 440 Stainless Steel offered by Continental Steel meets or exceeds some of the toughest standards including ASTM, QQ, and MIL-S.
Standard Size of our stainless steel flat bar
| Standard | ASTM A276-06 | |||||
| Size Specification | 3×20 | 5×40 | 8×20 | 10×60 | 15×50 | 20×60 |
| 3×25 | 5×50 | 8×25 | 10×80 | 15×60 | 20×80 | |
| 3×30 | 5×60 | 8×30 | 10×100 | 15×80 | 20×100 | |
| 3×40 | 5×80 | 8×40 | 12×20 | 15×100 | 25×40 | |
| 3×50 | 5×100 | 8×50 | 12×25 | 16×30 | 25×50 | |
| 4×20 | 6×20 | 8×60 | 12×30 | 16×40 | 25×60 | |
| 4×25 | 6×25 | 8×80 | 12×40 | 16×50 | 25×70 | |
| 4×30 | 6×30 | 8×100 | 12×50 | 16×60 | 25×100 | |
| 4×40 | 6×35 | 10×20 | 12×60 | 16×70 | 30×40 | |
| 4×50 | 6×40 | 10×25 | 12×80 | 16×80 | 30×50 | |
| 4×60 | 6×50 | 10×30 | 12×100 | 16×100 | 30×60 | |
| 5×20 | 6×60 | 10×35 | 15×20 | 20×30 | 30×80 | |
| 5×25 | 6×80 | 10×40 | 15×30 | 20×40 | 30×100 | |
| 5×30 | 6×100 | 10×50 | 15×40 | 20×50 | ||
Our Stainless Steel Flat Bar Pictures




Hot Tags: 440a 440b 440c stainless steel flat bar stock high hardness, China 440a 440b 440c stainless steel flat bar stock high hardness suppliers, Stainless Steel 446 Round Bar, 304 304L 316 316L Stainless Round Bar, 420 Stainless H type Steel, Stainless Steel 310S Round Bar, 304 316 Steel Flat Bars With Holes
You Might Also Like
Send Inquiry