Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel plate alloy 347/347h in China. If you're going to wholesale high quality stainless steel plate alloy 347/347h made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Available thicknesses for Alloy 347/347H:



| 3/16" | 1/4" | 5/16" | 3/8" | 1/2" | 5/8" | 3/4" | 7/8" | 1" | 1 1/8" |
|---|---|---|---|---|---|---|---|---|---|
| 4.8mm | 6.3mm | 7.9mm | 9.5mm | 12.7mm | 15.9mm | 19mm | 22.2mm | 25.4mm | 28.6mm |
| 1 1/4" | 1 1/2" | 1 3/4" | 2" | 2 1/4" | 2 1/2" | 2 3/4" | 3" | 3 1/2" | 4" |
| 31.8mm | 38.1mm | 44.5mm | 50.8mm | 57.2mm | 63.5mm | 69.9mm | 76.2mm | 88.9mm | 101.6mm |
Alloy 347 stainless steel plate exhibits good general corrosion resistance that is comparable to 304. It was developed for use in the chromium carbide precipitation range of 800 – 1500°F (427 – 816°C) where un-stabilized alloys such as 304 are subject to intergranular attack. In this temperature range, the overall corrosion resistance of Alloy 347 stainless steel plate is superior to Alloy 321 stainless steel plate. Alloy 347 also performs somewhat better than Alloy 321 in strongly oxidizing environments up to 1500°F (816°C).
The alloy can be used in nitric solutions, most diluted organic acids at moderate temperatures and in pure phosphoric acid at lower temperatures and up to 10% diluted solutions at elevated temperatures. Alloy 347 stainless steel plate resists polythionic acid stress corrosion cracking in hydrocarbon service. It can also be utilized in chloride or fluoride free caustic solutions at moderate temperatures.
Alloy 347 stainless steel plate does not perform well in chloride solutions, even in small concentrations, or in sulfuric acid.
Fabrication Data
Alloy 347 stainless steel plate can be easily welded and processed by standard shop fabrication practices.
Cold Forming
The alloy is quite ductile and forms easily.
Hot Forming
The high sulfur content of Alloy 303 also has a detrimental impact on hot workability. If hot forming is required, once again, 304 should be considered as an alternate selection.
Machining
The cold work hardening rate of 347 stainless steel plate makes it less machinable than 410 stainless steel, but similar to 304. The table below provides relevant machining data.
Physical Properties
Density
0.288 lbs/in3
7.96 g/cm3
Specific Heat
0.12 BTU/lb-°F (32 – 212°F)
500 J/kg-°K (0 – 100°C)
Modulus of Elasticity
28.0 x 106 psi
193 GPa
Thermal Conductivity 200°F (100°C)
133 BTU/hr/ft2/ft/°F
16.3 W/m-°K
Melting Range
2550 – 2635°F
1398 – 1446°C
Electrical Resistivity
72 Microhm-cm at 20°F
FAQ
1.Q: Are you a factory or trading company?
A: We are professional manufacturer, and our company also is a very professional a trade company for steel products.We can provide a wide range of steel products.
2.Q:What do your factory do regarding quality control?
A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.
3.Q: Can I get samples before order ?
A: Yes, of course. Usually our samples are free. we can produce by your samples or technical drawings.
4.Q:How do you make our business long-term and good relationship?
A:We keep good quality and competitive price to ensure our customers benefit ; We respect every customer as our friend and we sincerely do business and make friends with them. No matter where they come from.
Hot Tags: stainless steel plate alloy 347/347h, China stainless steel plate alloy 347/347h suppliers, 400 2 4360 Alloy Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, Corrugated SS Roof Sheet, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS431 Stainless Steel Plate, SS410 Stainless Steel Plate
You Might Also Like
Send Inquiry