Type 420 Long Radius Pulled Tube Elbows
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of type 420 long radius pulled tube elbows in China. If you're going to wholesale high quality type 420 long radius pulled tube elbows made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Products Description
The Characteristic of 420 Stainless Steel
- Higher carbon content, which optimizes strength and hardness characteristics.
- It has the highest hardness of all stainless steel, with 12% chromium.
- The highest corrosion resistance is reached only in a fully hardened condition.
- Ideal for applications requiring high hardness.
Products Properties
Type 420 Long Radius Pulled Tube Elbows Physical Properties
SS 420 stainless steel physical properties are listed in the table below such as density, melting point, specific heat, electrical resistivity, elastic modulus, thermal conductivity, and coefficient of thermal expansion (CTE).
| SS 420 Physical Properties | |
| Density, g/cm3 (lb/in.3) | 7.8 (0.28) |
| Melting point, °C (°F) | 1450-1510 (2650-2750) |
| Specific heat capacity, J/kg · K (Btu/lb · °F) | 460 (0.11) at 0-100 °C (32 to 212 °F) |
| Electrical resistivity, μΩ·m | 0.55 at 20 ℃ |
| Elastic modulus (Modulus of elasticity), GPa (106 psi) | 200 (29.0) |
| Thermal conductivity, W/m · K (Btu/ft · h · °F) | 24.9 (14.4), at 100 ℃ (212 °F) |
| Coefficient of thermal expansion, μm/m · °C (μin./in. · °F) | 10.3 (5.7), at 0-100 ℃ (32-212 °F) |
| 10.8 (6.0), at 0-315 ℃ (32-600 °F) | |
| 11.7 (6.5), at 0-538 ℃ (32-1000 °F) | |
|
420 Grade Chemical Compositions |
||||||
Grade |
C | Mn | P | S | Si | Cr |
| 420 (1.4021) | 0.20 | 1.0 max | 0.04 max | 0.03 max | 1.0 max |
13.0 |
| 420 (1.4028) | 0.30 | 1.0 max | 0.04 max | 0.03 max | 1.0 max |
13.0 |
| 420 (1.4034) | 0.46 | 1.0 max | 0.04 max | 0.03 max | 1.0 max |
13.0 |
Type 420 Long Radius Pulled SS Pipe Fittings

Stainless steel grades that are similar to grade 420 stainless steels include martensitic steels such as the other versions of grade 420, having vanadium, sulphur and molybdenum in their composition, and the grade 440 series. Non-standard grade 420C has carbon content that is little higher than that of grade 420.
Martensitic stainless steels are ones with high hardness and high carbon content. These steels are generally fabricated using methods that require hardening and tempering treatments. The operating conditions of martensitic steels are affected by loss of material's strength at high temperatures, and decrease in ductility at negative temperatures.
Customer Case

FAQ
Q:What are your payment terms?
A:30% T/T in advance and 70% balance before shipment or based on BL copy or LC at sight.
Q:What about product pricing information?
A:Prices vary due to changes in raw material prices on a regular basis.
Q:Is it possible to send samples?
A:Of course, we offer free samples and express shipping to customers all over the world.
Q:Do you offer a service for customized products?
A:Yes, we can produce according to your specifications and drawings.
Q:Can I pay you a visit at your factory?
A:Customers from all around the world are welcome to visit our factory.
Q:Can you assist me in importing steel products for the first time?
A:Yes, we have shipping agent who will arrange the shipment with you.
Q: What is your delivery time?
A:Within 7 working days after receiving your balance payment.
Hot Tags: type 420 long radius pulled tube elbows, China type 420 long radius pulled tube elbows suppliers, 310 Butt Weld Flanges, Super Duplex Steel UNS S32750 Angle