Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 316/316l stainless steel angle in China. If you're going to wholesale high quality 316/316l stainless steel angle made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
316/316L Stainless Steel Angle
Product Details
316/316L (UNS S31600 & S31603) belong to the American standard austenitic stainless steel, the implementation standard: ASTM A276/A276M-2017.
Due to the addition of molybdenum, 316 stainless steel has excellent corrosion resistance, atmospheric corrosion resistance and high temperature strength, and can be used under harsh conditions; it has excellent work hardening (non-magnetic). As a low-carbon series of 316 steel, 316L stainless steel has the same characteristics as 316 steel, and has excellent grain boundary corrosion resistance.
Mainly used for: equipment used in sea water, chemical, dye, paper, oxalic acid, fertilizer and other production equipment; photography, food industry, coastal facilities, ropes, CD rods, bolts, nuts.
|
Stainless Steel Profiles Data Sheet |
|
| Product Name |
316/316L Stainless Steel Angle Bar, Equal & Unequal Angle Bars |
| Equivalent Materials |
316: UNS S31600/DIN 1.4401/AISI 316/SAE 316/SUS316/06Cr17Ni12Mo2 316L:UNS S31603/EN 1.4404/AISI 316L/SAE 316L/SUS316L/022Cr17Ni12Mo2 |
| Type | Cold drawn, hot rolled, forged |
| Shape | Triangle / Hexagonal / Square bar / Flat Bar / Angle Bar / H/I Beam / U Channel |
| Standard | GB,AISI,ASTM,DIN,EN,JIS |