Stainless 904L Steel Coil
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless 904l steel coil in China. If you're going to wholesale high quality stainless 904l steel coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
904L stainless steel is a type of high-end austenitic stainless steel coil that is widely used in various industries due to its outstanding corrosion resistance and durability. It is a superalloy capable of withstanding harsh environments, including seawater and acidic solutions.

Compared with traditional stainless steel grades, 904L stainless steel offers higher strength, heat-resistance, and toughness, making it an ideal material for applications that require superior performance. It is commonly used in chemical processing equipment, heat exchangers, and pharmaceutical equipment due to its excellent resistance to stress-corrosion cracking and pitting.
| Specification | Description |
|---|---|
| Thickness Range | 0.3mm - 12.0mm |
| Width Range | 1000mm - 2000mm |
| Coil Weight | 1 - 10 tons |
| Coil ID | 508mm or 610mm |
| Surface Finish | 2B, BA, No.4, HL, brushing, etc. |
| Standard | ASTM, ASME, EN, DIN, JIS |
| Tolerance | Thickness +/- 0.03mm; Width +/- 5mm |
| Chemical Composition | C ≤ 0.020, Si ≤ 1.00, Mn ≤ 2.00, P ≤ 0.045, S ≤ 0.035, Cr 19.0 - 23.0, Ni 23.0 - 28.0, Mo 4.0 - 5.0, Cu 1.00 - 2.00 |

In addition to its exceptional physical properties, 904L stainless steel coils also have a beautiful appearance, making them a popular choice for architectural and decorative applications. Its unique properties make it an incredibly versatile material that can be used in a broad range of industries.
Overall, 904L stainless steel coils are an excellent choice for applications that require both high strength and outstanding corrosion resistance. Its unique properties make it a strong competitor in the high-end stainless steel market, and its performance is well worth the investment. With unparalleled corrosion resistance and durability, it's no wonder that 904L stainless steel coils are becoming more and more popular among advanced industries and discerning customers.