Inconel 600 Alloy Aerospace Tube
Powder:Not Powder
Transport Package::Standard
Outside Diameter:6.0mm to 1219mm
Thickness:0.5mm to 100mm
Application areas: Automobile, petrochemical, industrial, aerospace, energy
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 600 alloy aerospace tube in China. If you're going to wholesale high quality inconel 600 alloy aerospace tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel 600 alloy is widely used in the aerospace field, mainly used to manufacture key components such as high-temperature turbine parts, combustion chambers and nozzles.
Inconel 600 alloy tube is mainly composed of nickel, chromium and iron, and has good high-temperature corrosion resistance and oxidation resistance. In addition, it has satisfactory thermal strength and high plasticity below 700°C, and is suitable for various hot and cold processing and welding processes.
Specifications of Inconel 600 Fabricated Pipes
Mechanical Properties
| Temper | Annealed | |
|---|---|---|
| Tensile Rm | 110 | ksi (min) |
| Tensile Rm | 738 | MPa (min) |
| R.p. 0.2% Yield | 37 | ksi (min) |
| R.p. 0.2% Yield | 255 | MPa (min) |
| Elongation (2" or 4D gl) | 45 | % (min) |
Physical Properties (Room Temperature)
| Specific Heat (0-100°C) | 460 | J.kg-1.°K-1 |
| Thermal Conductivity | 14.8 | W.m -1.°K-1 |
| Thermal Expansion | 12.4 | μm/μm/°C |
| Modulus Elasticity | 207 | GPa |
| Electrical Resistivity | 10.3 | Ohm-cm |
| Density | 8.42 | g/cm3 |
Chemical Composition (% by weight)
| Element | Min | Max |
|---|---|---|
| C | - | 0.15 |
| Si | - | 0.5 |
| Mn | - | 1 |
| S | - | 0.015 |
| Cr | 14 | 17 |
| Cu | - | 0.5 |
| Fe | 6 | 10 |
| Ni | 72 |
Nickel Alloy 600 Seamless Pipe Round Tube

Why choosing GNEE
Gnee has 14 steel production lines, 10 processing equipment for processing, bending, coating, heat treatment, cutting, drilling, beveling, tempering, surface treatment, etc., complete testing equipment and strong technical force. The annual production capacity is more than 60,000 tons, and it can implement GB, ASTM, JIS, DIN and other standards.
please contact us for a quote! ss@gneesteel.com
Latest technology inconel alloy 625 testing

Professional nickel-based alloy steel bars supplier-GNEE

GNEE PACKAGING AND SHIPPING

FAQ
Q. What are your company's main products ?
A: Our main products are stainless steel , carbon steel , galvanized steel, aluminium products , etc.
Q. How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS Verified.
Q.Is Inconel 600 better than hastelloy?
A.Inconel and Hastelloy are both nickel-chromium-molybdenum-based alloys. They are all corrosion-resistant and extremely strong metals. Hastelloy has greater molybdenum content than Inconel, although Inconel has a higher chromium concentration.
Hot Tags: inconel 600 alloy aerospace tube, China inconel 600 alloy aerospace tube suppliers, high temperature alloy, inconel alloy modulator parts, 706 602ca Inconel Alloy Pipe, inconel alloy combustion chamber parts, inconel alloy capacitor parts, inconel alloy exhaust system parts
You Might Also Like