Incoloy Alloy 890 Pipe
video

Incoloy Alloy 890 Pipe

Incoloy Alloy 890 (UNS N08890) is a high performance, heat resistant nickel-based alloy that maintains high strength at temperatures up to 2200°F (about 1200°C) and has excellent resistance to oxidation, carburization and sulfidation. This alloy is enhanced by increasing the content of molybdenum, silicon and niobium, making it a preferred material for extreme high temperature environments.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 890 pipe in China. If you're going to wholesale high quality incoloy alloy 890 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

INCOLOY alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with excellent resistance to oxidation, carburization, and sulfidation at temperatures up to 2200°F (1200°C).

Physical Properties

Density g/cm3 7.94
lb/in.3 0.287
Melting Range °F 2388 - 2522
°C 1309 - 1383

Mechanical Properties

Product Temper Temperature
°F (°C)
0.2% Yield
Strength, ksi (MPa)
Ultimate Tensile
Strength, ksi (MPa)
Elongation Reduction of
Area, %
Hot-Rolled Plate Solution-Annealed 72 (22) 39.4 (272) 94.5 (652) 46.6 62.7
Cold-Drawn Tubing Solution-Annealed 72 (22) 48.4 (334) 94.2 (652) 46.5 60.1
Hot-Rolled Plate Solution-Annealed 1600 (870) 16.0 (110) 23.5 (132) 84.8 71.0
Hot-Rolled Plate Solution-Annealed 1800 (980) 9.6 (66) 13.4 (92) 98.0 87.5
Hot-Rolled Plate Solution-Annealed 2000 (1100) 6.4 (44) 9.0 (62) 83.6 91.8

 

376377378