Hastelloy N
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy n in China. If you're going to wholesale high quality hastelloy n made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
HASTELLOY® N alloy (UNS N10003) is a nickel-base alloy that was invented at Oak Ridge National Laboratories as a container material for molten fluoride salts. It has good oxidation resistance to hot fluoride salts in the temperature range of 1300 to 1600°F (704 to 871°C).
In tests of over two years duration, corrosion attack on HASTELLOY® N alloy in molten fluoride salts at temperatures up to 1300°F (704°C), was less than one mil per year. It is expected that alloy N will be most useful in environments involving fluorides at high temperatures; however, the alloy compares favorably with other HASTELLOY® alloys in various corrosive media, as shown in the table of penetration rates. Corrosion test samples of the alloy are available from Haynes International locations. It is especially suggested that the alloy be tested in molten halides of zirconium, beryllium, lithium, sodium, potassium, thorium or uranium.
HASTELLOY® N alloy has good oxidation resistance in air. It shows promise for continuous operations at temperatures up to 1800°F (982°C). Intermittent use at temperatures up to 1900°F (1038°C) may also be possible. No discernible oxidation could be measured for the alloy at temperatures up to 1200°F (649°C).
Metallographic examinations have shown that the elements in alloy N remain in solid solution in the 1100 to 1600°F (593 to 871°C) range. Tensile tests have indicated no tendency toward embrittlement for prolonged periods at 1500°F (816°C). Alloy N has good weldability and can be readily forged. The hot working range is between 1600 and 2150°F (871 to 1177°C). It has been successfully extruded and further processed into high-quality seamless or manufactured as welded and drawn tubing.
Solution heat-treatment is recommended after hot or cold working of HASTELLOY® N alloy parts. For sheet and plate, this is accomplished by soaking at 2150°F (1177°C) [sections up to 1/4 inch thick] and then cooling rapidly in air, or at 2165°F (1185°C) [sections 1/4 inch and thicker] followed by waterquenching. HASTELLOY® N alloy can be supplied, to order, in the forms of sheet, plate, and bar. HASTELLOY® N alloy sheet, plate, bar, rod, and welded and seamless wrought pipe and tubing have been approved for use in the construction of unfired pressure vessels in accordance with the requirements of the ASME Boiler and Pressure Vessel Code Section VIII under Case 1315 (Special Ruling). Alloy N is approved for use at temperatures up to 1300°F (704°C). Design data can be found here.
More +
Main Standards




Chemical Composition
Data Sheet
Physical Properties
| Density | g/cm3 | 8.86 | |
|---|---|---|---|
| lb/in.3 | 0.320 | ||
| Melting Range | °F | 2375 - 2550 | |
| °C | 1300 - 1400 | ||
Mechanical Properties
| Form | Condition | Aging Temperature | Test Temperature | Tensile Strength | Yield Strength (0.2% Offset) |
Elongation | ||
|---|---|---|---|---|---|---|---|---|
| 0.063 in thick | Heat-treated for at 2150°F (1177°C), RAC | °F | °C | °F | °C | psi | psi | % |
| - | - | RT | RT | 115,100 | 45,500 | 50.7 | ||
| - | - | 1100 | 593 | 86,900 | 32,900 | 45.3 | ||
| - | - | 1300 | 764 | 69,600 | 31,600 | 30 | ||
| - | - | 1500 | 816 | 55,900 | 29,500 | 24.3 | ||
| - | - | 1700 | 927 | 34,000 | 25,900 | 30 | ||
| - | 1500 | 128 | RT | RT | 115,400 | 49,300 | 46.8 | |
| Heat-treated at 2150°F (1177°C), then welded and tested as-welded | - | - | RT | RT | 116,100 | - | 37.5 | |
| - | - | 1200 | 649 | 71,500 | - | 17 | ||
| - | - | 1300 | 704 | 63,500 | - | 10.5 | ||
| - | - | 1500 | 816 | 52,000 | - | 8.5 | ||
| Sheet 0.045 in thick | Heat-treated at 2100°F (1177°C), RAC | - | - | RT | RT | 114,400 | 44,700 | 50 |
| - | - | 1000 | 538 | 93,000 | 28,300 | 46 | ||
| - | - | 1100 | 593 | 93,000 | 28,900 | 50 | ||
| - | - | 1200 | 648 | 82,400 | 27,500 | 37 | ||
| - | - | 1300 | 704 | 69,900 | 28,000 | 24 | ||
| - | - | 1400 | 760 | 61,800 | 26,200 | 21 | ||
| 1000 | 10,000 | RT | RT | 117,700 | 45,100 | 50 | ||
| 1100 | - | RT | RT | 120,000 | 47,500 | 49 | ||
| 1200 | - | RT | RT | 116,000 | 46,800 | 46 | ||
| 1300 | - | RT | RT | 115,500 | 45,800 | 46 | ||
| 1400 | - | RT | RT | 115,000 | 43,600 | 40 | ||
| 1000 | 10,000 | 1000 | 538 | 97,700 | - | 46 | ||
| 1100 | - | 1100 | 593 | 90,500 | - | 40 | ||
| 1200 | - | 1200 | 649 | 81,900 | - | 32 | ||
| 1300 | - | 1300 | 704 | 76,100 | - | 24 | ||
| 1400 | - | 1400 | 760 | 65,100 | - | 20 | ||
| Weld Metal | As Welded | - | - | RT | RT | 116,100 | - | 39.3 |
| - | - | 1200 | 649 | 73,600 | - | 18.1 | ||
| 1200 | 500 | RT | RT | 116,800 | - | 38.6 | ||
| - | - | 1200 | 649 | 82,700 | - | 26.5 | ||
FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.